A Fractographical Study on Dissimilar Weld Joints of SAF 2205 and Hastelloy C-276


Creative Commons License

Çelikkol E., TÜMER M., ATAPEK Ş. H., Kerimak M. Z.

5th International Conference of Engineering Against Failure, ICEAF-V 2018, Chios, Yunanistan, 20 - 22 Haziran 2018, cilt.188, (Tam Metin Bildiri)