Microstructural characterization of carbides in a cast high-speed steel using different metallographie techniques Mikrostrukturelle charakterisierung von carbi-den in einem schnellarbeitsstahlguss anhand verschiedener metallographischer verfahren


Creative Commons License

Gümüş S., Atapek Ş. H., Polat Ş., Erişir E., Alkan A.

Praktische Metallographie/Practical Metallography, cilt.49, sa.12, ss.767-781, 2012 (SCI-Expanded, Scopus)

Özet

High-speed steels are mostly manufactured by casting and they exhibit a characteristic dendritic microstructure with primary carbides In this study, the morphology of carbides in a cast high-speed steel is investigated using light and scanning electron microscopes. The morphology and structure of the carbides were revealed by means of different metallographic techniques such as chemical and electrolytic etching and color metallography. The combination of these metallographic techniques gives different approaches to how different primary carbide morphologies can be observed in the martensitic structure. Besides, microa-nalysis was carried out to determine the chemical composition of primary carbides using SEM/EDX. © Carl Hanser Verlag, München Pract. Metallogar.