Experimental and modelling investigations on effect of initial microstructure and aluminide coating thickness on high temperature oxidation of MAR-M247 nickel-based superalloy


Piotrowska K., Bochenek K., Włoczewski M., Aktaş Çelik G., Yılmaz Güler F. B., Atapek Ş. H., ...Daha Fazla

Journal of Alloys and Compounds, cilt.11, ss.1-20, 2026 (Scopus)