Effect of Carbon Fiber, Graphene Nanoplatelet, and Chain‐Extender Reinforcement on the Hygrothermal Durability of 3D‐Printed PLA Composites: A Combined Mechanical and Thermal Study


Karslı Yılmaz N. G., Yılmaz T., Fidan S., Özsoy M. İ., Ürgün S., Bora M. Ö.

Polymer Composites, ss.1-29, 2026 (Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1002/pc.71885
  • Dergi Adı: Polymer Composites
  • Derginin Tarandığı İndeksler: Scopus
  • Sayfa Sayıları: ss.1-29
  • Kocaeli Üniversitesi Adresli: Evet

Özet

Hygrothermal durability of FDM printed polylactic acid (PLA) composites containing short carbon fiber (CF, 3 wt%), graphenenanoplatelets (GnP, 0.5 wt%), and epoxy-functional chain extender (Joncryl, 0.1 wt%) was studied. Printed filaments obtainedusing two-step extrusion were exposed to up to 400 freeze-heat cycles from −20°C to +40°C at 93% relative humidity and fur-ther analyzed through gravimetric, tensile, DSC, and SEM studies. Whereas the GnP additive caused the maximum moistureuptake of 0.336%, the uncompatibilized hybrid of CF and GnP demonstrated a non-monotonic behavior (moisture uptake reached0.400% at 200 cycles, but dropped to 0.143% at 400 cycles) with temporary loss of mechanical performance and presence of in-terphase cavities (image analysis: 51 cavities mm−2 , 19.9% area fraction, equivalent diameter up to 127 μm). Incorporation ofJoncryl prevented any increase of moisture uptake (0.179%), avoided any loss of strength during aging, maintained ductility, andproduced the highest strength (51.48 MPa) and stiffness (4173.3 MPa) after 400 cycles. Factorial ANOVA showed formulationto be the main factor (about 50% of the variance for strength and 61% for modulus), with a secondary, non-monotonic effect ofaging; the formulation × aging interaction was not statistically significant. Within the investigated formulations and exposureconditions, the Joncryl-modified composite was the most hygrothermally stable.